First time I brewed NPP I couldn't get it to fully dissolve and it was weaker but still good.
I use a .25 or .22-20. Sterile of course.
I don't disagree gentle heating is a good idea for bonding but I don't agree with the high temp. I have seen flash coil heating as an element of bonding.
I have not seen it in brews and the highest I ever go is 200 degrees for 10-20 min.
Im not saying some don't do it in a controlled manner such as flash coiling but its not something I would do since melting raws can degrade and the solvents start to breakdown and condensate at that temp as well. Not to mention BA will flash burn at 300 degrees.
So that's interesting..thanks for that info
I use a .25 or .22-20. Sterile of course.
I don't disagree gentle heating is a good idea for bonding but I don't agree with the high temp. I have seen flash coil heating as an element of bonding.
I have not seen it in brews and the highest I ever go is 200 degrees for 10-20 min.
Im not saying some don't do it in a controlled manner such as flash coiling but its not something I would do since melting raws can degrade and the solvents start to breakdown and condensate at that temp as well. Not to mention BA will flash burn at 300 degrees.
So that's interesting..thanks for that info